Me yasa aka yi wa centrifuges ado da HALAR?
1. Juriyar zafin jiki mai yawa (matsakaicin zafin aiki 150℃);
2. Ƙarfin juriyar acid da alkali (ƙimar PH tsakanin 1~14)
3. Mannewa mai kyau (matsi mara kyau na iya kaiwa 0.09Mpa, tasirin injin)
4. Tsawon rai na sabis (shekaru 8 zuwa 10 a ƙarƙashin yanayi na yau da kullun, garantin gabaɗaya yana da iyaka ga shekara 1)
5. Ƙarfin juriya ga shigar ciki (hydrofluoric acid, chlorine gas, bromofluoric acid da sauran iskar gas suna da kyakkyawan juriya ga shigar ciki)

Babban fasali:
Kayayyakin da centrifuge ya raba duk suna da tsatsa har zuwa wani mataki, kuma kayan da suka taɓa kayan dole ne su cika buƙatun juriyar tsatsa don tabbatar da amfani mai lafiya.
Ire-iren kayan gini: 304, 321, 316L, 904L, farantin titanium, bakin karfe mai duplex, da sauransu.
Matakan maganin lalata saman: rufin PE, rufin roba, fesa HALAT, da sauransu.
Ya kamata kwastomomi su sanar da masana'anta game da halayen zahiri da na sinadarai (halayen sinadarai, zafin jiki yayin rabuwa, da sauransu) na kayan da ruwan wanke-wanke da tsaftacewa, don masana'anta su iya ba da shawarar zaɓar kayan centrifuge bisa ga halayen matsakaicin da aka raba, da kuma saita zoben rufewa, gaskets da yadudduka masu tacewa don tabbatar da buƙatun hana lalata na centrifuge.
Me yasa taurin saman rufin yake da mahimmanci?
Saboda taurin saman da ya fi girma yana samar da:
Inganta juriya ga lalacewa (kamar yawan zubar da abubuwa da gogayya na ƙwayoyin cuta ko gishiri da ake amfani da su)
Inganta juriyar karce (misali a guji lalacewa yayin shigarwa)
Wannan ya sa ECTFE ya zama babban abin da ke ƙara aminci. A lokacin shigarwa da jigilar kaya, ana rage yiwuwar lalacewa ta zobe ba zato ba tsammani kuma ana rage farashin kulawa.
Me yasa santsi na fenti yake da mahimmanci?
Fuskar Halar ECTFE, ko an fitar da ita, ko an yi mata fenti ko kuma an shafa mata foda, tana da santsi sosai, kamar yadda aka tabbatar ta hanyar duba na'urar auna hasken lantarki ko na'urar auna hasken lantarki ta hanyar amfani da ...
Amfanin saman da ya yi santsi
Yana rage yiwuwar samun ramuka a cikin rufin
Yana hana tarin ƙwayoyin halitta masu ƙarfi da gishirin ƙarfe kuma yana hana toshewar abubuwa, wanda ya fi bututun PP, PVC ko FRP kyau.
Rage samuwar biofilm da ƙwayoyin cuta, sakamakon biofilm ɗin ya nuna idan aka kwatanta da ƙarfe mai laushi da sauran ƙwayoyin fluoropolymers.